Isotropic Finishing

Category
Name
Isotropic Finishing
Category
Note
No metallurgical degradations such as hydrogen embrittlement and/or intergranular corrosion.
Increased resistance to contact fatigue and bending fatigue.
Generates surfaces up to Ra 0.025. That’s the best we’ve done.
Increased allowable power density.
Elimination of micro-pitting.
Increased scuffing resistance.
Reduced friction and wear.
Increased lubricant performance.